FLAIR® Air Flame Treatment

Corona & Plasma Treatment: FLAIR for a BOPP line by Plasmawerk Germany
  • Ultra high surface tension
  • Long lasting treatment
  • High energy efficiency
  • Durable stainless steel roller
  • Compact size
  • Reliable plasma/corona technology

Marketing Potentials

  • creates significant competitive advantage for BOPP and CPP producers by smart use of well known plasma technology
  • directly reduces running costs and downtimes
  • opens new market potentials
  • easy to install in existing lines: perfect upgrade
Corona / Plasma Treatment – FLAIR in a CPP line by Plasmawerk Germany

For further information please contact us at sales@plasmawerk.de

Best Practice

Parameters Case 1

Requirements of the customer:

  • Material: PP, non-conductive
  • Application: FLAIR plasma treatment in a cast film system
  • Treatment width/pages to be treated: 2,850 mm / 1-sided
  • Production/max. machine speed: 300 m/min / max. 500 m/min
  • Height inlet/outlet: 2.210 / 500 mm
  • Material thickness: 12 – 250 μm

Supplied Features:

  • Generator power: 50 kW
  • Electrode type: FLAIR
  • Roll surface: stainless steel
  • Plasma dose: 58.5 Wmin/m2 at 300 m/min
  • Achievable surface tension: 52 mN/m.

Parameters Case 2

Requirements of the customer:

  • Material: PP backsheet foil and others other non-conductive foils
  • Application: single/double-sided FLAIR treatment in a blown film line
  • Treatment width/pages to be treated: 2,200 mm / 1(2)-sided
  • Production/max. machine speed: 15 m/min / n.n.
  • Material thickness: 360 µm and thinner

Supplied Features:

  • Generator power: 2x 10 kW
  • Electrode type: FLAIR, segmented, grid 8 mm
  • Roll surface and diameter: stainless steel, 200 mm
  • Plasma dose: 300 Wmin/m² at 15 m/min
  • Achievable surface tension: 72 mN/m on the backsheet film, measured according to ISO 8296 or FINAT FTM 15 Series A or B, max. 60 minutes after treatment under laboratory condition 23/50 according to ISO 291.